+49 441 94986-0

Information about tests

tear resistance (also folded edges), (temperature range -40 to +120 °C)

methods available: trapezoid, Trouser, on request: FhG leaflet 6 part 9 (folded edges- trapezoide, extra charge!), Graves

test method:Mechanical/ technological properties
Norms: DIN 53363 (2003-10)
DIN ISO 34-1 (2004-07)
ASTM D 1938 (2019)
DIN EN ISO 6383-1 (2016-05)
FhG Merkblatt 6 Teil 6 (1987)
Needed sample size:sample over total width of material, min length: 0,5 m

Standardprüfungen

tear strength DIN EN ISO 6383-1 (trouser test, sample width 50 mm)
Quasistastic test method by using a tensile tester, suitable for characterisation of all rigid and soft plastic films up to 1 mm thickness. Not suitable for brittle materials. Can also be carried out in the thermal chamber.
Norm: DIN EN ISO 6383-1


tear strength of folded edges, trapezoid- method
Quasistatic test method by using a tensile tester, particularly suitable for characterisation of the resistance of folded edges of flexible films. Not suitable for brittle materials. Can also be carried out in the thermal chamber.
Norm: FhG Merkblatt 6 Teil 6


tear strength -Graves
Quasistastic test method by using a tensile tester,particularly suitable for characterisation of elastomeric- films or - sheet up to 1 mm thickness. Not suitable for brittle materials. Can also be carried out in the thermal chamber.
Norm: DIN ISO 34-1


tear strength- trapezoid
Quasistastic test method by using a tensile tester, suitable for characterisation of all rigid and soft plastic films up to 1 mm thickness. Not suitable for brittle materials. Can also be carried out in the thermal chamber.
Norm: DIN 53363




back to overview Mechanical/ technological properties

Search examinations


Your contact person

Matthias Böhne +49 441 94986-11
matthias.boehne@innoform.de