tensile test paper, sealing strength of paper samples

paper DIN EN ISO 1924-2 determination of tensile strength, stretch at break,TEA (accredited test method) DIN EN 868-4 Anhang C, Measuring the seal strength of machine-made bags or sealed samples made of paper

test method:Mechanical/ technological properties
Norms: DIN EN 868-4-C (2017-05)
DIN EN ISO 1924-2 (2009-05)
DIN ISO 3781 (2012-07)
Needed sample size:sample over total width of material, min length: 0,5 m; min ca. 150 mm sealing/ welded seam

Standardprüfungen

seal strenght DIN EN 868 part 4 appendix C - paper bags
Packaging for terminally sterilized medical devices- paper bags
Norm: DIN EN 868 Teil 4 Anhang C (DIN EN ISO 1924-2)


tensile test Paper and board - standard
Norm: DIN EN ISO 1924-2




back to overview Mechanical/ technological properties